Skip to first unread message

Shihabuddin Ramli

unread,
Jul 5, 2015, 10:48:46 AM7/5/15
to material...@googlegroups.com

Can anybody explain to me why its stated in latest API660 for this requirement? Its not stated any reason why is shall be PWHT due to lethal sevice or regarding thickness

Shiha

Hemant Solanki

unread,
Jul 6, 2015, 4:16:26 AM7/6/15
to material...@googlegroups.com
in 6 or more passes there will be more welding on surfaces within close proximity. Such welding will make parent metal hard and brittle... in order to avoid such problem, PWHT requirement is added by API, so that parent metal becomes soft and adhere to its properties.

Shihabuddin Ramli

unread,
Jul 6, 2015, 9:15:55 AM7/6/15
to material...@googlegroups.com

Any precaution need to be taken during pwht, especially to avoid any distortion? We have faced a problem before that after pwht, the bonnet was leak at the flange joint after installed and need to be clamped, tq in advance sir

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/121d03d5-1651-4eb2-b5c3-a7c8797c9703%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages