API 570 SHORT TERM CORROSIN FORMULA CHANGE FEB-2016

42 views
Skip to first unread message

Mohd Siraj

unread,
Nov 25, 2016, 9:30:34 PM11/25/16
to Materials & Welding
DEAR ALL,

REFER API 570 2009 VERSION AND API570 FEB2016 VERSION,
SHORT TERM CORROSION FORMULA IS CHANGED??

AS PER API-570 2009,
ST=       tprevios-tactual
               -------------------------
        time (years) t previous-t actual

AS PER API-570 2016,
ST=           t inital-t actual
              -----------------------------
        time (years) t previos-t actual 

pl confirm this change in equation.

Sathish Kumar

unread,
Nov 28, 2016, 9:34:45 PM11/28/16
to material...@googlegroups.com
Dear Siraj,
Yes, it was changed. Please refer to the attached.

Regards,

Sathish K
Cswip3.1, API510
Jazan, KSA.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/11981924-a60d-47a4-b0ef-986d70a96763%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

API570- 2016.bmp
Reply all
Reply to author
Forward
0 new messages