Can we use Duplex WPS for Super Duplex, kindly quote with the help of codeThanks
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ee5dcbf4-b6cb-4421-8338-04e109d45b15n%40googlegroups.com.
Can we use Duplex WPS for Super Duplex, kindly quote with the help of codeThanks
--
Can we use Duplex WPS for Super Duplex, kindly quote with the help of codeThanks
--
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ90KGR%2BWjiOTHjPf4mNLed34QHj4QP3_KD%2BzfeckX20tFydUA%40mail.gmail.com.
ASME Section IX groups materials by P-Numbers to control essential variables.
Duplex Stainless Steels (e.g., UNS S31803 / S32205)
→ P-No. 10H
Super Duplex Stainless Steels (e.g., UNS S32750 / S32760)
→ P-No. 10I
📌 Since P-No. 10H ≠ P-No. 10I, they are treated as different base material groups.
ASME Section IX clearly states:
QW-403.11
A change from one P-Number to another P-Number is an essential variable and requires requalification of the WPS.
✅ Therefore:
A WPS qualified on Duplex (P-No. 10H)
Cannot be used for Super Duplex (P-No. 10I)
Without a new PQR covering P-No. 10I
Although not strictly required by code, this reinforces why the rule exists:
Super Duplex has:
Higher PREN
Higher yield and tensile strength
Tighter control on heat input, interpass temperature, and ferrite/austenite balance
Welding Super Duplex with a Duplex-qualified WPS risks:
Loss of corrosion resistance
Sigma phase formation
Improper phase balance
Codes intentionally separate these alloys due to these risks.
Even if a Super Duplex filler metal is used, the limitation still applies, because:
QW-404 (Filler Metal Essential Variables)
Filler metal control does not override base material P-Number limitations.
❌ A Duplex WPS cannot be used for Super Duplex welding.
✅ ASME Section IX requires requalification, because:
Duplex = P-No. 10H
Super Duplex = P-No. 10I
Change in P-Number is an essential variable per QW-403.11
Can we use Duplex WPS for Super Duplex, kindly quote with the help of codeThanks
--
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADkb7FDnfAUxq4kw9%3DUhUQrskiz5oSv1%2Bdh1yqHMs3ygzx-Epg%40mail.gmail.com.

To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHXTn13GP75Hk7hisbt4yD5v5brzSvKEUfseobmjDxGf6JqYNQ%40mail.gmail.com.
Thanks & Regards
J.Gerald Jayakumar
0091-8838619635