Rechniques for checking internal surface of piping 12" and 16" for natural gas supply

63 views
Skip to first unread message

Mohammed Ghani

unread,
Feb 15, 2015, 7:15:41 AM2/15/15
to material...@googlegroups.com
Dear Experts,

please let me know there is any technique available for checking internal surface of piping (in service fuel natural gas)

And also if there is nay technique for checking internal surface of piping during shutdown please let me know.
Thanks and Regards, ?

Mohammed Ghani,

CSWIP 3.1 / BGAS L-2 / ISO 9001:2008 QMS LA.

Mechanical Inspector,
BUREAU VERITAS.


ü
 Please consider the environment before printing this email.

 "Be the change you wish to see in the world"

---Mahatma Gandhi---

Kunal Patel

unread,
Feb 15, 2015, 1:20:14 PM2/15/15
to material...@googlegroups.com
Dear friend,

For checking internal surface of piping, we can use Borescope or Fiberscope. This is an instrument, which is available in market or vendor places.

Regards,
Kunal Patel
BVIS Ahmedabad.

smkabeer ahamed

unread,
Feb 15, 2015, 11:11:30 PM2/15/15
to material...@googlegroups.com
Dear friend,

snake eye -iii is one type of instrument  used to check internal surface defects,welding defects.vt-level-ii engineers used that instrument.you can approach ndt agency to collect  that instrument and inspect that piping.

Thanks and regards.

S.M.Kabeer ahamed
chief engineer
M/S.QUEST -BANGALURU
INDIA


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2a5bc249-f4b9-4c05-9b56-db67ce9d0598%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.


Mohammed Ghani

unread,
Feb 16, 2015, 12:59:30 AM2/16/15
to material...@googlegroups.com
Dear,

its a 40 mtr. continous in service pipe line. i need two options.

1. with out shutdown any chances of internal surface inspection?.
2. with shutdown what are the various types of instruments available for checking internal surface of piping of 40 mtr. length.

Thanks and Regards,
Mohammed Ghani.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

For more options, visit https://groups.google.com/d/optout.



--

Umar Rashid Makrani

unread,
Feb 16, 2015, 12:59:37 AM2/16/15
to material...@googlegroups.com
Dear Sir,
You can use UT thickness survey and LiXi profiling to monitor the piping while in service. Once offline, during shutdown Boroscopes may be used.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.

Umar Rashid Makrani

unread,
Feb 16, 2015, 2:30:27 AM2/16/15
to material...@googlegroups.com
for a continuous pipeline you can use LRUT online and again boroscope offline.

 
With Best Regards,
Umar Rashid Makrani, PMP® ,
 API653, NACE CIP-2, LEEA Registered Engineer.

Tadic, Miroslav

unread,
Feb 18, 2015, 8:29:06 AM2/18/15
to material...@googlegroups.com

Hello

 

You can use a NDT technique called ultrasound guided waves (UTGW)

 

This technique can detect a serious kind of defects in pipelines, internal and external. Depending of pipe conditions, this NDT can inspect even 50 meters of pipeline in just one test.

 

As is based in ultrasonic principle, this use longitudinal and torsional waves to detect indications which are categorized quantifying the transversal loss of area in pipe. As complement, then you can use single beam of ultrasonic thickness measure to check any indication

 

This can be used with pipeline in service

 

Attached you can find a little information about this NDT

 

There are a lot of services in NDT which offer this one

 

Regards     

 

Miroslav Tadic
Ingeniero  de Integridad
CEE
Gerencia de Producción - Mantenimiento
YPFB Chaco S.A.

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.