NDE rate in boiler

30 views
Skip to first unread message

Zakaria ghrab

unread,
Oct 12, 2016, 5:00:12 AM10/12/16
to material...@googlegroups.com
Dear Experts,

  Need your assistance.

Applicable code : ASME sect I
Query : 

1- For Pipes/tubes NPS less than 4" diameter, we need to perform NDE with some ratio, basically according code is not mandatory (table PW-11) : Please inform if any other indication about this issue in code.

2- Could us perform NDE (RT : Volumic) before pwht and complete only by (MT: Surfasic) after pwht for P91 and also for others grades according ASME sect I. What's code requirement for NDE/Pwht.
tat 

--

Thanks and Regards, 

Vishwas Keskar Welding Manager Pune India

unread,
Oct 12, 2016, 11:59:06 PM10/12/16
to Materials & Welding
nps < 4 " = if RT  is taken, the acceptance shall be as per written down RT PROCEDURE 
 
P91 - RT BEFORE AND AFTER BOTH is required as a good eng practice

Kannayeram Gnanapandithan

unread,
Oct 13, 2016, 12:41:22 AM10/13/16
to materials-welding
As per B 31.1, NDE after any Heat treatment

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Wed, Oct 12, 2016 at 10:07 PM, Vishwas Keskar Welding Manager Pune India <vvkes...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (vvkes...@gmail.com) Add cleanup rule | More info

nps < 4 " = if RT  is taken, the acceptance shall be as per written down RT PROCEDURE 
 
P91 - RT BEFORE AND AFTER BOTH is required as a good eng practice

On Wednesday, October 12, 2016 at 2:30:12 PM UTC+5:30, Tunisian Quality Engineer wrote:

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0bcbf00a-f553-4d85-8d42-28452834ef0e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages