We have project need to weld Everhard C400 to SS304. Please give me a hint on welding electrode to use, ER309 is a good choice?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0b795cbe-87b4-4e85-b599-30e63532fe91n%40googlegroups.com.
We have project need to weld Everhard C400 to SS304. Please give me a hint on welding electrode to use, ER309 is a good choice?
--