Dear all
 can you please  tell   the qualification deposit limit for fillet weld: max size deposit for single pass and min size deposit for multi pass as per aws d1.1

saeed sarir

unread,
May 5, 2023, 1:11:57 AM5/5/23
to material...@googlegroups.com
Hello
you can to use of table
Best regards

Saeed Sarir
IKA Technical Inspector
ASNT-Level II in PT,MT & UT
Phone number : +98 09132387465

Thank you for thinking of the environment before printing this email.  
One tree can start a forest.



On Wed, May 3, 2023 at 9:25 AM Sayyed Aneesh <sayyeda...@gmail.com> wrote:
Dear all
 can you please  tell   the qualification deposit limit for fillet weld: max size deposit for single pass and min size deposit for multi pass as per aws d1.1

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0b027691-f4c2-4ff1-aeec-44082a81484en%40googlegroups.com.
AWS D1.1 2020.pdf
Reply all
Reply to author
Forward
0 new messages