PSV Testing

33 views
Skip to first unread message

chiluka venkatramulu

unread,
Dec 23, 2019, 10:08:36 PM12/23/19
to materials-welding
Dear All,
If PSV having flange rating 300 X 600, which rating is considered for testing Body & Bonnet, as per B16.34.

With Best Regards,
Venkatramulu CH

Eyup Tan

unread,
Dec 23, 2019, 10:37:58 PM12/23/19
to material...@googlegroups.com
#600 rating because #600 flange for inlet and #300 is for outlet (exhaust) flange

Regards 
Eyup Tan

iPhone’umdan gönderildi

chiluka venkatramulu <ramulu...@gmail.com> şunları yazdı (24 Ara 2019 06:08):


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF98%2BdEjRwiKGN8%3DoE-Zqih6F-pDD_KfRr-4QB2ZUEX%2BHoD9gw%40mail.gmail.com.

chiluka venkatramulu

unread,
Dec 24, 2019, 12:23:32 AM12/24/19
to materials-welding
Can you give me any code reference pl.

Regards,
Venkatramulu CH

Eyup Tan

unread,
Dec 24, 2019, 3:39:06 AM12/24/19
to material...@googlegroups.com
API 526
2.3 Valve Selection
For valves described in this standard, inlet and outlet
flange sizes and pressure-temperature ratings shall conform
to the data in Tables 2 through 15 for spring-loaded valves
and Tables 16 through 29 for pilot-operated valves. Inlet and
outlet pressure limits are governed by the flange
pressure/temperature limits or by the manufacturer’s design
limits, whichever is lower.


Saygılarımla, / Best Regards,

Eyup Tan



Johnson Madukayil

unread,
Dec 28, 2019, 3:49:02 AM12/28/19
to material...@googlegroups.com
Body and bonnet is tested at the outlet flange pressure rating.
Check ASME VIII-1 UG-136 d)2)

chiluka venkatramulu

unread,
Dec 30, 2019, 12:35:08 AM12/30/19
to materials-welding
I have checked  ASME VIII-1 UG-136 d)2)-it is not clear that  "Body and bonnet is tested at the outlet flange pressure rating."


Regards,
Venkatramulu CHILUKA

Reply all
Reply to author
Forward