Hi Zakaria,
You need to look under this chapter, chapter Off-white is all about Fusion of Plastics. Fusion not Welding is not the term used for joining of plastics.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent Consulting Welding & Metallurgical Engineering Specialist
Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)
Saudi Aramco Approved Designated Project Welding Engineer (DPWR)
Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
From: TQM <zakari...@gmail.com>
Sent: December 1, 2021 7:19 AM
To: Materials & Welding <material...@googlegroups.com>
Subject: HDPE pipe joint (welding), procedure and acceptance
Dears,
Could you please inform for HDPE pipes joining, if any Welding procedure is required (Is it mandatory as the steel welding case ?)
the inspection method ?
and the related code/ standard please.
Thank you.
Sorry for the typo, it should read as , Chapter QF. Joining of HDPE is covered under the requirements for polyethylene.
Thanks
P.Goswami, P.Eng, IWE.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAuAAAAAAAAABVPzeizzeRJsiPziIE5jXQBAMO2jhD3dRHOtM0AqgC7tuYAAAAAAA4AABAAAAA6tUBK9%2BWDR5Ny731HyHkyAQAAAAA%3D%40rogers.com.
Sorry for the typo, it should read as , Chapter QF. Joining of HDPE is covered under the requirements for polyethylene.
Thanks
P.Goswami, P.Eng, IWE.
From: material...@googlegroups.com <material...@googlegroups.com> On Behalf Of pgos...@rogers.com
Sent: December 1, 2021 8:19 AM
To: 'TQM' <zakari...@gmail.com>
Cc: 'Materials & Welding' <material...@googlegroups.com>
Subject: [MW:32626] RE: HDPE pipe joint (welding), procedure and acceptance
Hi Zakaria,
You need to look under this chapter, chapter Off-white is all about Fusion of Plastics. Fusion not Welding is not the term used for joining of plastics.
Thanks.
Pradip Goswami.P.Eng, IWE.
Independent Consulting Welding & Metallurgical Engineering Specialist
Consultant: SNC Lavalin Inc. (Nuclear &Non-Nuclear)
Saudi Aramco Approved Designated Project Welding Engineer (DPWR)
Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.
Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/
Email:pgos...@rogers.com,pradip....@gmail.com
Cell/Whasapp:1-905-9793232
<image001.png>
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0655b142-a5e8-49de-858d-978316cbe548n%40googlegroups.com.