Dear Sir,
I have a 2 chemical compositions one is Italian material another one is Brazilan material, Requesting you to conform the grade or any equivalent material in Indian grade.
Italy chemical composition
ELEMENTS % BY WT
C 0.243
Si 0.26
Mn 1.19
P 0.012
S 0.008
Cr 0.32
Ni 0.16
Mo 0.05
HARDNESS HRC: 43.7
Brazil chemical composition
ELEMENTS % BY WT
C 0.183
Si 0.80
Mn 1.34
P 0.026
S 0.014
Cr 0.14
Ni 0.11
Mo 0.04
HARDNESS HRC: 41.7
Anyone Please help me....
Regards
Vinay