Dear All,
Please clarify for electrode qualification test as per ASME Sec II Part C for E7018 Dia-4 mm, what are the test requirements?.
As per Table 4, Fillet weld test piece is required for chemical analysis, RT, All-weld test & Impact test. Please clarify what table 4 is stating.
Further, if i make one Groove weld test assembly of 20 mm thick, is it sufficient for the electrode qualification?
Thanks & Regards,
Mohan Raj