I need solution for two issues
1.We are using IS 2062 E-410 Grade material , for that E-7018 electrode is enough?
2.For welding chequered plate can we select E-6010 over e-6013?

vaishakh

unread,
May 21, 2019, 5:34:17 AM5/21/19
to Materials & Welding
Dear Experts,
 
         Currently we are using E-7018 electrode to weld IS 2062 E-410BR grade material.Please tell me wheather this electrode is enough to weld this grade material or should i go for E-8018. Please help me to solve this.
Thanks and Regards
Vaishakh.k.c.


rakesh kasera

unread,
May 22, 2019, 5:10:13 AM5/22/19
to Materials & Welding
Hi

U can use E7018 

Regards

Rakesh Kasera


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01e6f607-15c0-4a1f-a4e4-a0f45c85f872%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Vinay Thattey

unread,
May 22, 2019, 5:10:15 AM5/22/19
to material...@googlegroups.com
Should be OK

pradip kumar Sil

unread,
May 22, 2019, 8:30:48 AM5/22/19
to materials-welding
E-6013 is enough

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

pradip kumar Sil

unread,
May 22, 2019, 8:30:48 AM5/22/19
to materials-welding
You can use E-7018, E-6010 & E-6013 according to service requirement