Hi,
It will not qualify…
As F no & A No are not only the criteria for acceptance…
F&A grouping are majorly for welder / operator qualification and not to consider in PQR.
Need to go for a fresh PQR.
Thanks & Regards,
Lakshman Kumar B,
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83ce3674-8b7a-42d2-b8f6-98aa0cdb35db%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83ce3674-8b7a-42d2-b8f6-98aa0cdb35db%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83ce3674-8b7a-42d2-b8f6-98aa0cdb35db%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/008701d1ef9a%2486d40920%24947c1b60%24%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
F&A nos not essential for welding operators
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/83ce3674-8b7a-42d2-b8f6-98aa0cdb35db%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/008701d1ef9a%2486d40920%24947c1b60%24%40gmail.com.
| From: Kannayeram Gnanapandithan Sent: Σάββατο, 6 Αυγούστου 2016 - 16:20 To: materials-welding Reply To: material...@googlegroups.com Subject: Re: [MW:25207] RE: 25195] PQR Qualification. |
I have mentioned only welding operator to whom fno is not essential. Pl ref QW361.1&.2
Wrong F no is essential for performance qualificationSent from my BlackBerry 10 smartphone.
From: Kannayeram GnanapandithanSent: Σάββατο, 6 Αυγούστου 2016 - 16:20To: materials-welding
Reply To: materials-welding@googlegroups.com
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOF7OM237Ok%2B7xpTW196AJOnAE%2Be5aD2XG3tM0ZLdr5Yg%40mail.gmail.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160806150955.6713426.97455.3994%40gmail.com.