WPS for SAW

199 views
Skip to first unread message

Lakshman

unread,
Mar 15, 2016, 5:49:36 AM3/15/16
to material...@googlegroups.com

Hi friends,

 

I want a WPS (incl PQR) for the following parameters, if anyone is having, please share it, it will help us a lot for me…

 

Material – IS 2062 (or Pno 1)

Thickness – above 20mm.

Process – SAW – (No SMAW, No Tig and etc)

Joint configuration – Square butt, both sides welding.

Application – pipe welding (manufacturing at factory)

 

Thanks in advance for the cooperation.

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

Alan Denney

unread,
Mar 15, 2016, 10:20:42 AM3/15/16
to material...@googlegroups.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/001401d17e93%24a8709da0%24f951d8e0%24%40com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

Lakshman Kumar B

unread,
Mar 15, 2016, 10:55:10 AM3/15/16
to material...@googlegroups.com
Its not for a LSAW, it's for spiral welded pipe, and also its for a water service application not for Oil&Gas,

Lakshman kumar.B
Project manager.
9440031459

From: Alan Denney
Sent: ‎15-‎03-‎2016 19:50
To: material...@googlegroups.com
Subject: [MW:24530] RE: 24528] WPS for SAW

pgoswami

unread,
Mar 15, 2016, 12:11:57 PM3/15/16
to material...@googlegroups.com

Hello Lakshman,

 

Square butt SAW on 20 mm (3/4”) thick would be difficult some chamfer or Vee-Prep would be required. This technique is perfectly feasible for @  ½”   thickness. Please see this online handbook from EASB for more guidance.

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

H-905-6799677, 905-9631505

C-905-9793232

 

 

http://www.esabna.com/euweb/sa_handbook/585sa2_27.htm

 


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/56e82228.61f8420a.6f908.ffffef39%40mx.google.com.

Lakshman Kumar B

unread,
Mar 15, 2016, 11:31:49 PM3/15/16
to material...@googlegroups.com
Hi Goswami, thanks a lot fir the info, however in one of my earlier site I welded with square but for 18mm double side SAW weld, however I lost that data, some of the water sector teams might have the data, and I am looking for the same.



Lakshman kumar.B
Project manager.
9440031459

From: pgoswami
Sent: ‎15-‎03-‎2016 21:41
To: material...@googlegroups.com
Subject: [MW:24532] RE: 24531] RE: 24530] RE: 24528] WPS for SAW

[The entire original message is not included.]

anosh wankhade

unread,
Mar 16, 2016, 12:44:20 AM3/16/16
to material...@googlegroups.com
Dear Laxman,

For IS pipes you can follow IS 7307 for WPS/PQR.
But You can not do welding of 20 mm and above with square butt, double V groove can give you satisfactory results.Tandem arrangements will be needed for the same.
Rest all parameters and essential variable you can find in IS 7307.
You can get format of WPS/PQR in IS 7307 OR ASME Section IX

Regards,

Anosh Wankhade.
8959591446
Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

Kannayeram Gnanapandithan

unread,
Mar 16, 2016, 12:44:35 AM3/16/16
to materials-welding
upto 16mm in wind mill done, but heavy current is required and second side there will back grinding for 2mm for visibility


THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY