Circumferential pipe weld joint resting on structural beam in process piping

798 views
Skip to first unread message

Biplab Pal

unread,
Mar 28, 2017, 11:22:00 AM3/28/17
to materials-welding
Dear experts,

We need your kind support based on your experience and any code/std references.

The situation is that some of our process piping in refinery division THE CIRCUMFERENTIAL JOINT has come such position that the joint rests on the structural beam.
Is it allowed?

Some inspector have a concern that there is a developed stress while operation and the joint may fail.

Please share your experience and reference.

Thank you very much 

With best regards
Biplab Pal
--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

M.Sathiya Narayanan

unread,
Mar 29, 2017, 11:16:29 PM3/29/17
to material...@googlegroups.com
generally touching is not allowed, however  you can find the solution from client spec itself 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFnzQg22xWSiTOEonpZtZCDqBZ9vvh9OGZ_bKvHJ9CrS1L-qSg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Thanks and Regards
M.Sathyanarayanan

Prasad Rode

unread,
Mar 29, 2017, 11:18:13 PM3/29/17
to Materials & Welding
Dear sir,

You can avoid such type of issue by internal drawing study.

Secondly, Do the RT of the joint and make it flush and place a shoe support below it.
In second option, you can also cut the pipe and place a piece of pipe in between shoe.
In second case , your one extra joint will be created but no issue of failure in future.
In third option, you can shift the pipe and make the joint safe.


Regards
Prasad

Perumal Govindan

unread,
Mar 30, 2017, 11:22:09 PM3/30/17
to material...@googlegroups.com

Hi

Please adjust the pipe support location after approval by your piping design engineering and if not possible to adjust get concurrence from them for close out.

Regards
P Govindan

--

jaya anil

unread,
Mar 31, 2017, 12:02:43 AM3/31/17
to material...@googlegroups.com
Generally,  piping drawings shall take care of this type of issues during fabrication of pipe spools. 

It is a very common problem, if you don't have any option to move the support,  then before the support cut and add one pup piece pipe and do all welding and NDT as per the  regulations  and avoid the fouling. 



Regards
Anil 

--

bijoy.joseph1

unread,
Apr 1, 2017, 3:08:00 AM4/1/17
to Perumal Govindan, material...@googlegroups.com
1. Grind the pipe joint reinforcement on the contact area of beam.
2. Do NDT on the joint.
3. Get the design approvel.



Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: Perumal Govindan <perumal...@gmail.com>
Date: 03/30/2017 7:02 PM (GMT+03:00)
Subject: Re: [MW:26328] Circumferential pipe weld joint resting on structural beam in process piping

Hi

Please adjust the pipe support location after approval by your piping design engineering and if not possible to adjust get concurrence from them for close out.

Regards
P Govindan

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9e%2BGe67n6SNt%3DUtPKfxxQpEUS7iTagBbxO5YqSLv6jL0A%40mail.gmail.com.

dilintas

unread,
Apr 1, 2017, 3:08:03 AM4/1/17
to material...@googlegroups.com
It is not prohibited
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

J.J. Thomas.

unread,
Mar 12, 2019, 11:17:03 AM3/12/19
to Materials & Welding
Dears. Can any one provide an industrial std reference?

munee...@gmail.com

unread,
Mar 15, 2019, 11:02:03 AM3/15/19
to materials-weldingmaterials-welding
Allowed if your owner allows with a mutal agreement that cap passes will be flushed off and NDE will be done to make sure that zero imperfections, our cases we welded wear pads flusing off cap passes followed by PT / RT or UT.

Thanks.


Regards,
MOHAMED MUNEEB MAHABOOB


---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages