I am trying to locate an S-N diagram for a sintered tungsten powdered
alloy with the following general characteristics:
90% W + 10% Cu-Ni-Fe
Density 16.85 - 17.25 g/cc
Rc hardness = 32 max.
UTS 120 ksi (827 MPa) min.
YTS 80 ksi (551 MPa) min. (0.2% offset)
Elongation 10% min in 1" gage length.
I have an application with a 400 MPa fluctuating stress, and I am trying
to establish the endurance limit for the above material to determine if
there is infinite life. Any information would be helpful. Thank You,
Ed Carlson
(313) 995-1755Carls...@aol.com