The adhension of Cr film on lithium niobate

0 views
Skip to first unread message

sduio...@gmail.com

unread,
Sep 6, 2008, 4:48:04 AM9/6/08
to
I have some problem in Sputtering Cr film on lithium niobate
substrate. The adhension of sputtered Cr film is bad and cannot stand
the wet etching process. Is andbody know the answer?
I would appreciate any input.