Both symptoms point to air leak in the chamber, causing oxidation of the
newly deposited film and drifting of the pressure. Try leak checking the
chamber prior to turning the power on first, and then with the power on to
verify its integrity. An RGA would be useful because it will tell you
what's going on in there real time. I'd also increase the vacuum some to
improve the film quality. Hope this helps.
Anco Blazev
<lsudh...@googlemail.com> wrote in message
news:fa2f4a6b-3862-40cd...@d77g2000hsb.googlegroups.com...