ive finished up my 50lb sack and my supplier cant get anymore///
tia,
Moose,
Moose Studios pottery
>anybody know of a bulk supplier for borate?
>
>ive finished up my 50lb sack and my supplier cant get anymore///
>
Have you tried other borates? I've been happy
with Gillespie Borate as a direct substitute for
Gerstley. There are a few others out there (whose
names don't come to mind just now) that might also
work, possibly with some recipe modifications. If
you can get a decent analysis of whatever brand
you end up with, you can probably use any glaze
program to make the tweaks.
Best regards,
Bob Masta
DAQARTA v4.51
Data AcQuisition And Real-Time Analysis
www.daqarta.com
Scope, Spectrum, Spectrogram, Sound Level Meter
FREE Signal Generator
Science with your sound card!
I heard Laguna Clay is trying to re-open the mine. You might try their
web site.