dished head shape for 2: 1 elleptical dished head

29 views
Skip to first unread message

asad azmi

unread,
Feb 17, 2012, 7:57:05 AM2/17/12
to material...@googlegroups.com
Dear All,
 
Greetings.
 
A dished head of  ID 1520 mm & thk 80 mm hot formed by subcotractor. A vessel is being manufactured by ASME SEC VIII DIV1.
as per the forming report  dished head is having Overcrowning of 10 mm & SF is 70 mm.
 
 Now vessel manufacturer  is claming that Dished is having 10 mm plus side SF( 80 mm). manufacturer wants to shift tan line by 10 mm to maintain overall lenght.
 
my question is --
 
1)  is it mandatory that for  for a dished having overcrowing,  SF  will also be more than required.
 
2) what is the effect on Knuckle radius if the SF is shifted by 10mm.( considering the fact that contractor  has  done forming of the dished head considering 70 mm SF).
 
3) can we accept the dished head if  dished head forming contactor certify that even with 80MM SF the true shape of  the dished head will be satisfactory.
 
can we accept the dished head if  true shape of the  dished head  is checked by a template( 2: 1 elleptical type) which is having 80mm SF & it is showing satisfactory result.
 
Please advice.
 
Thanks & Regards
 
Asad Azmi
 
 

manjunath madiwalar

unread,
Feb 18, 2012, 2:21:09 AM2/18/12
to material...@googlegroups.com
Hi,

if SF is more you are adjusting overal lenghth & template is
suiting there is no problem with dish.

Regards.

Manjunath

On 2/17/12, asad azmi <azmias...@gmail.com> wrote:
> Dear All,
>
> Greetings.
>
> A dished head of ID 1520 mm & thk 80 mm hot formed by subcotractor. A
> vessel is being manufactured by ASME SEC VIII DIV1.
> as per the forming report dished head is having Overcrowning of 10 mm & SF
> is 70 mm.
>
> Now vessel manufacturer is claming that Dished is having 10 mm plus side
> SF( 80 mm). manufacturer wants to shift tan line by 10 mm to maintain
> overall lenght.
>
> my question is --
>
> 1) is it mandatory that for for a dished having overcrowing, SF will
> also be more than required.
>
> 2) what is the effect on Knuckle radius if the SF is shifted by 10mm.(
> considering the fact that contractor has done forming of the dished head
> considering 70 mm SF).
>
> 3) can we accept the dished head if dished head forming contactor certify
> that even with 80MM SF the true shape of the dished head will be
> satisfactory.
>

> *can we accept the dished head if true shape of the dished head is


> checked by a template( 2: 1 elleptical type) which is having 80mm SF & it

> is showing satisfactory result.*


>
> Please advice.
>
> Thanks & Regards
>
> Asad Azmi
>

> --
> To post to this group, send email to material...@googlegroups.com
> To unsubscribe from this group, send email to
> materials-weld...@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

Reply all
Reply to author
Forward
0 new messages