ThicknessRange of wps

90 views
Skip to first unread message

israr ahmed

unread,
Jun 27, 2025, 11:55:53 PM6/27/25
to material...@googlegroups.com


dear team
What should be the range of qualification if we are welding sight glass thickness 40mm with shell of 10mm?

Israr Ahmed Noor Mohammed
+919930308261

Pravin Kurade

unread,
Jun 28, 2025, 4:03:03 AM6/28/25
to material...@googlegroups.com
In this case it's dissimilar thickness and considering its P8 you need 20 mm thk welding procedure which will cover both the range I assume impact test not required. 
Thanks with Regards....

Pravinkumar Kurade

ASME Authorized Inspector (National Board-15396), 
Repair Inspector (NBIC) R-Endorsement,
PED Inspector, DOSH Inspector,
B.E. (Mech.), Lean Six Sigma Green Belt,
C-SWIP-3.1 (Welding Inspector - UK)
ASNT Level II - MT, PT, RT , VT, LT

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEJoza%2Bw8YOMSuBzMnVCePwFuvbJDVm6AtKDh0AhGZtmpqTHmw%40mail.gmail.com.

Michael Tino

unread,
Jun 28, 2025, 5:40:01 AM6/28/25
to material...@googlegroups.com
If it’s P8, won’t a PQR qualified on 6mm thick cover the welding of this dis-similar thickness (QW-202.4)considering welding deposit thickness of 10mm?
 Regards,
Michael 