                     We have repair in Golden joint and it is successfully done. But now client is asking for penalty for this joint as it was a 5% RT line.
But as per my understanding as it is a Golden Joint ( a 100% RT joint), so no need of repair penalty. But I am not getting any code reference to it. Please help me to find any reference.

Thanks and Regards,

Bishwambhar Kumar


Shashank Vagal

unread,
Aug 12, 2018, 10:18:05 PM8/12/18
to material...@googlegroups.com
In this case an additional NDT, say UT is advisable. Please discus with your client.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enq...@neometalanalystndt.com / nach...@yahoo.com




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

munee...@gmail.com

unread,
Nov 7, 2018, 7:46:57 AM11/7/18
to materials-welding
Explain your client that penalty comes under % coverage where there is a failure, when a weld is considered as mandatory RT 100 % it is like an additional joint and 100% services do not required any penalty regardless of lineclass.

If really you wanted to cover your lineclass then you wouldnt be giving golden joint as 100%.

It is to be understood.

Regards,
M.Muneeb.