Qualification of Square Tube As per ASME Section IX Edn 2023

43 views
Skip to first unread message

Netaji Rayate

unread,
Jun 25, 2025, 6:57:47 AM6/25/25
to Materials & Welding
Dear Members,
I require Qualification of Square Tube as per ASME section IX.
for Butt Joint Can we Consider Square Pipe as Round Pipe or tube for Diameter Limits as per ASME section IX 
 
for T joint in Square Tube to Plate, Can we use Square Tube  instead of round pipe for procedure Qualification as shown in figure.QW 462.4(d) ASME Section IX 

If yes,Please mention Reference & Thk ,Diameter Limits for same.

Thanks

Harish Gandhi

unread,
Jun 28, 2025, 2:18:05 AM6/28/25
to material...@googlegroups.com
In my opinion square tube / pipe shall be considered as plate welding which involves overhead, vertical and flat welding. Procedures qualifying above 
Positions and required thickness may be used for welding. In pipe welding direction for welding is continuously changing and requires more skill hence diameter limits are given in code.
Regards
 
Harish Gandhi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/f26f8c96-147c-4a38-9880-dc0c4f3aa08fn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages