Is postion consider an essential variable in WPS.
If I have a WPS in 4G postion can i use that WPS in 1g, 2G, 3G position..

Madheswaran s

unread,
Jun 30, 2024, 11:01:21 PM6/30/24
to Materials & Welding
Hi, welding position: Non-Essential for WPS as per ASME Sec IX code ., but essential variable as per AWS D1.1 code.