Procedure qualification and Performance qualification of a welder in fillet weld

79 views
Skip to first unread message

Saravanan Selvakumar

unread,
Feb 17, 2023, 3:23:53 AM2/17/23
to Materials & Welding
Hi all,

I did a procedure qualification with a 4" pipe and 150 mm plate in 5F position, as per ASME Sec IX QW-451.3 he is qualified to weld all base metal thickness and all diameters.

But for WPQT, he is qualified only for 73 mm and above pipes, does that mean i have to make another performance test for 1/2" and 1" pipes separate are is he qualified to do all size of pipes.

Kindly Clarify.

Regards,
Saravanan S.

james gerald

unread,
Feb 17, 2023, 11:31:48 PM2/17/23
to 'Saravanan Selvakumar' via Materials & Welding
Yes for welder performance qualification for lower diameters as given in QW-452 shall be qualified.

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8b8814ab-9094-483b-ada5-91ac2863cc5en%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages