Welding procedure with Impact test

103 views
Skip to first unread message

Somu Meganathan

unread,
Oct 11, 2017, 6:37:26 AM10/11/17
to Materials & Welding
Hello all,

Till  today we have not qualified any welding procedures with impact test requirements. Now we got an order with impact test requirements. i.e, HE body flange need to be impact tested at -9 deg. C. It seems we need to qualify the welding procedures with impact test.

My doubts are We need to qualify the welding procedure with impact with -9 Deg.C or can we do less than -9 Deg.C. Is it required impact tested welding procedures, when the materials need impact test qualified?

Regards,
M.SOMU
 

james gerald

unread,
Oct 11, 2017, 7:19:26 AM10/11/17
to material...@googlegroups.com
It depends on the Materials(Grade) and P. No Grades & Group No & Design Code to determine the Weld Impact tests. Please provide

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Tamizh Selvan

unread,
Oct 11, 2017, 7:36:07 AM10/11/17
to material...@googlegroups.com
It is an supplementary essential variable ... so need to perform impact test .

With Warm Regards,

S.TAMIZH SELVAN,
Mobile: +91-9597370860 ( India )
          

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Dinesh Somwanshi

unread,
Oct 11, 2017, 10:23:37 PM10/11/17
to materials-welding
Dear ,

It is depend on material MOC, While you no need to qualify full procedure again you may proceed only with Impact Testing keeping parameters within earlier qualified WPS.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

Mhaskar Aly

unread,
Oct 12, 2017, 10:58:44 PM10/12/17
to material...@googlegroups.com
Yes.. WPS to be qualified with impact test; if you have PQR suitable for BM, FM is suitable for impact properties , welded in uphill positions  and tested for code required tests, then you need to weld only one test coupon as per existing WPS & carry out impact test at MDMT or lower temp.

When Design specify applicability of impact test, then you need your welding procedures with impact test.

Aly

--
Reply all
Reply to author
Forward