Dear Experts ,
If the wleder is qualifide for 6G test , can he weld the plate of unlimited thickness ?
or he needs to Qualify 4G test to weld unlimited thickness of plate ?
wether the 6G welder is sapose to weld only pipes.
awaiting for welding experts valueable suggestions ..........
Regards ABDUL JABBAR KHAN |
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Hi,
If the welder qualified in 6G position with the pipe thickness(test specimen) is more than 13mm,then he qualified for pipe and plate of maximum to be welded.
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282 --- On Mon, 8/1/11, Biplab Pal <bipla...@googlemail.com> wrote: |