I have query regarding application A106 specification.

In the old edition of Astm A106 - edition 99 and  latest SA106 specification, there is a clause for Additional requirements of yield strength as per A 520 shall be followed in case the product to be used in application confirming to  ISO recommendations of Boiler Construction.

1 )Can anyone explain me the definition / scope of  ISO recommendations of Boiler construction ?

also. As per current ASTM revisions,  standard A520 has made Obsolete &  the clause of additional requirements for ISO recommended Boiler construction has been removed in revised edition of A106 - edition. 2009.

now to design pipe class according to ASME 31.3 , do I have to consider any additional requirement ?

One of the reply from Lloyds NOBO. was to follow yield strength  as per ASME section II part D table Y-1.

Then for calculations , which allowable stress value shall be consider , ASME 31.3 table A-1  or  ASME Se. II part D, table 1A ?

kindly advise me on the matter.


Kind regards

Rahul

nandakumar pandit

unread,
Nov 23, 2009, 9:16:20 AM11/23/09
to material...@googlegroups.com
Drar Rahul

While designing pipeline you can consider the values given in ASME Se. II part D, table 1A,
as same values are also considered in designing neck thickness of a nozzle, which normally is made from a pipe.

Regards
nspandit

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Pisat, R. R(ahul)

unread,
Nov 24, 2009, 5:55:30 AM11/24/09
to material...@googlegroups.com
Hello Mr. Nandkumar,
 
Thank you for your reply,
but I am designing pipe class for petrochemical plant and not PIPE LINE, as per ASME B31.3
Allowable strees from ASME B31.3 are different than ASME Se. II part D, table 1A. and they are according to ASME Se. II part D, table 2A.
 
ASME Se. II part D , Table 1A has more conservative allowable stresses with 3.5 desing factor for SMTS.
Why should I design pipe class under ASME 31.3 code , with design stress from ASME Sec. II table 1 A .
 

Kind regards

Rahul Pisat
Piping Specialist
Plant Design

Akzo Nobel Technology & Engineering B.V.
Postal address: PO Box 9300, 6800 SB  Arnhem, the Netherlands
Visiting address: Velperweg 76, 6824 BM Arnhem, the Netherlands

T +31 26 366 4706, F +31 26 366 3401,
Visit our website @ www.akzonobel.com/te  

 


From: nandakumar pandit [mailto:pand...@gmail.com]
Sent: maandag 23 november 2009 15:16
To: material...@googlegroups.com
Subject: Re: [MW:3716] scope of ISO Recommendations for Boiler Construction...

____________________________________________________________________________
This email has been scanned for Viruses and Spam. For more information
please contact your local Business Unit Information Security representative.
____________________________________________________________________________
Reply all
Reply to author
Forward
0 new messages