Which Filler wire to be used in between P43 (Inconel 625) to P8 (A240 310S) by GTAW)

457 views
Skip to first unread message

rahmat khan

unread,
Nov 23, 2021, 3:44:21 AM11/23/21
to Materials & Welding
Dear All,

Please help me with this:

1) which filler wire is to be used for GTAW welding of two dissimilar materials P number that is P43 (Inconel 625) to P8 (A240 310S).

2) For SA 516 Gr 70 22mm thick. Ellipsoidal 2:1 dish end, which heat treatment to be used as per ASME Sec VIII Div I UCS 56 After cold forming of dish end.

Please help me I this?

 

Arun Padman

unread,
Nov 23, 2021, 4:12:59 AM11/23/21
to material...@googlegroups.com
Dear,

For welding  Inconel 625 to 310 you can use ER NiCrFe-2 or-3.

Regards,

Arun Padman Manayil

P  Save a tree. Please don't print this e-mail unless you really need to



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/441df1fa-c04c-4f4a-a027-af6c169e7cc3n%40googlegroups.com.

rahmat khan

unread,
Nov 23, 2021, 10:19:47 PM11/23/21
to Materials & Welding
As per my understanding For P43 Filler wire ER NiCrMo-3 is suitable as per chemical and mechanical properties.

Kannayeram Gnanapandithan

unread,
Nov 24, 2021, 12:30:26 AM11/24/21
to materials-welding
inconel 625

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--

Arun Padman

unread,
Nov 24, 2021, 3:09:40 AM11/24/21
to material...@googlegroups.com
Dear,

ER NiCrMo-3 is suitable to weld 625 to 600/625/825/C-22/B-2 etc., not 310.

Regards,

Arun Padman Manayil
P  Save a tree. Please don't print this e-mail unless you really need to

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Kannayeram Gnanapandithan

unread,
Nov 24, 2021, 4:31:14 AM11/24/21
to materials-welding
Why Inconel 625 is not suitable, could you elaborate to understand.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

sajeed zaheer

unread,
Nov 24, 2021, 4:31:15 AM11/24/21
to material...@googlegroups.com
For the first point the filler you can used ER Ni cr Mo-3
For dish head after cold forming it depends  on fiber elongation of material usually 5 to 10 fiber elongation PWHT is required and above 10 Normalizing and tempering is required.

On Wed, Nov 24, 2021 at 6:19 AM rahmat khan <mkrahm...@gmail.com> wrote:
--

Babur Khan

unread,
Jun 25, 2023, 11:18:21 PM6/25/23
to material...@googlegroups.com
Greetings,
Please share WPS sample for P43 to P8 welding. 
ASME Sec. ix.

Muhammad Babur Khan
Sent from my iPhone

On 24 Nov 2021, at 12:31 PM, Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:



Sourav Bohray

unread,
Jun 25, 2023, 11:32:33 PM6/25/23
to material...@googlegroups.com


for dish head after cold forming heat treatment is not mandatory as per asme secVIII div1 untill you are not exempted from condition as per ug79,ucs79.
if not exempted than do heat treatment as per ucs56 called it stress relieving.

you have option of normalizing also for cold form dish head heat treatment but for that you need one copoun to be normalized and tested as per ug 85.

if dish head are welded than you need pqr with same heat tretament :-
if dish head is stress relieved- pqr also stress relieved
if dish head is normalized- pqr also normalized



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages