Dear Experts, 

Will CJP WPS qualify for Fillet Welds ?

Baqer Shabbeer

unread,
Jun 8, 2023, 2:27:04 AM6/8/23
to material...@googlegroups.com
Please share here qualification’s and design code

On Wed, 7 Jun 2023 at 1:58 PM, Parminder Singh <parms...@gmail.com> wrote:
Dear Experts, 

Will CJP WPS qualify for Fillet Welds ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8bee16cf-540c-431a-a8b2-b5409547abd1n%40googlegroups.com.
--
Regards,
Baqer Shabbeer

Parminder Singh

unread,
Jun 8, 2023, 2:43:09 AM6/8/23
to material...@googlegroups.com
WPS qualified in CJP as per AWS D1.1 Ed 2020 

james gerald

unread,
Jun 8, 2023, 8:05:11 AM6/8/23
to material...@googlegroups.com
Details like plate,  position etc.. required. Decode from the below snapshot of AWS D1.1

Inline image
Inline image



Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



mithlesh kumar

unread,
Jun 10, 2023, 8:08:05 AM6/10/23
to Materials & Welding
Dear James,

Attached table is for position qualification , Only in case of T,Y & K Type joint fillet can performed. Please correct me if I am wrong.


Thanks
Mithlesh

james gerald

unread,
Jun 11, 2023, 11:06:36 PM6/11/23
to material...@googlegroups.com
Just to add as per AWS D1.1 the weld types requiring qualification.


Inline image

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635

james gerald

unread,
Jun 11, 2023, 11:06:36 PM6/11/23
to material...@googlegroups.com
YES it is for the Applicable positions Qualified.

Fillet welds shall be Qualified Separately. If your question is whether CJP groove weld qualifies Fillet weld then is is NO.

Fillet test shall be qualified as below.

Inline image


Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-8838619635

On Saturday, 10 June, 2023 at 05:38:01 pm IST, mithlesh kumar <mithles...@gmail.com> wrote:


Naveen Kumar

unread,
Apr 18, 2024, 4:03:21 AM4/18/24
to Materials & Welding
CJP Groove qualify Fillet weld also.

Source:
AWS D1.1:2020 Section 6.12 Last Paragrapgh "Any PJP qualification shall also qualify any fillet weld size on any thickness"

My understanding is: 
As per sec 6.12.1 Qualified CJP PQR can Qualify PJP confirming to Fig 5.2, Now your CJP PQR is qualified for PJP, So Any PJP qualification shall also qualify fillet weld.

1.PNG