Welders Qualification

61 views
Skip to first unread message

YOUSIF YOUNIS

unread,
Jun 19, 2019, 2:37:08 AM6/19/19
to Materials & Welding
How can I now size of coupon for qualification depending on the thickness or diameter or together?
 

Kamal Basha

unread,
Jun 21, 2019, 12:14:41 AM6/21/19
to material...@googlegroups.com
Both together

On Wed, 19 Jun 2019, 9:37 a.m. YOUSIF YOUNIS, <q...@masco-iq.com> wrote:
How can I now size of coupon for qualification depending on the thickness or diameter or together?
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6232571c-513a-4a9f-9ca7-7daf240ab968%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Bien_ND

unread,
Jun 23, 2019, 10:57:25 AM6/23/19
to Materials & Welding
Follow standard application.
normally limit min. OD for welder and welding operator qualification.

Vinay Thattey

unread,
Jun 27, 2019, 6:17:29 AM6/27/19
to material...@googlegroups.com
It is the thickness , that matters.

On Wed, 19 Jun 2019 at 12:07, YOUSIF YOUNIS <q...@masco-iq.com> wrote:
How can I now size of coupon for qualification depending on the thickness or diameter or together?
 

--
Reply all
Reply to author
Forward
0 new messages