ASTM A216 Vs ASME SA216 Difference

4,512 views
Skip to first unread message

vijay frnds

unread,
Mar 9, 2010, 4:12:51 AM3/9/10
to material...@googlegroups.com
Dear friends,


I have received the customer order for pipeline valves with ASME SA216 Gr WCB.

My doubt is there any diff. between ASTM A216 Gr WCB Vs ASME SA216 Gr WCB.

Thank you,


--
Urs . . .
Muthu
Smile make(s)miles ! ! !
Please don’t print this e-mail unless you really need to! - this will preserve trees on our planet earth.

AGUSTIN JIMENEZ

unread,
Mar 9, 2010, 8:02:07 AM3/9/10
to material...@googlegroups.com, INSPECTORES DE EQUIPOS ESATICOS
Hi, there is not diff. between boths only A and SA, the standart is iqual, review in ASME Section 2 and ASTM.
 
Agustin


De: vijay frnds <frndst...@gmail.com>
Para: material...@googlegroups.com
Enviado: mar, marzo 9, 2010 4:42:51 AM
Asunto: [MW:4502] ASTM A216 Vs ASME SA216 Difference
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



¡Obtén la mejor experiencia en la web!
Descarga gratis el nuevo Internet Explorer 8
http://downloads.yahoo.com/ieak8/?l=e1

John Henning

unread,
Mar 9, 2010, 9:59:36 AM3/9/10
to material...@googlegroups.com
SA-216 states the following:  "Identical with ASTM Specification A216/A216M-07 except for the addition of 2.3 and editorial differences in 2.1 and 10.1."
 
2.3 references ASME Section IX
10.1 requires welders and welding procedures used for repair to be qualified in accordance with ASME Section IX
 
 2.1 - no significant difference that I could quickly discern
 
All else is the same.
 
John

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of vijay frnds
Sent: Tuesday, March 09, 2010 3:13 AM
To: material...@googlegroups.com
Subject: [MW:4502] ASTM A216 Vs ASME SA216 Difference

Arunachalam A

unread,
Mar 9, 2010, 11:15:30 AM3/9/10
to material...@googlegroups.com
if the item SA 216 is meant for code stamped vessels and parts, then the acceptable ASTM editions are upto 2007 editions ( check the table of acceptable ASTM Editions in Part II-A).
You need to check the material certificates, if the same is of ASTM. If ASTM is mentioned in the MTC, instead of SA, then ASTM EDITION Year need to be in Certificate.

arun
--
ARUNACHALAM.A
050-5257122

There are three types of people in the world,
First makes wonder happen,
Second see wonders happen and
Third one wonders what happened!

Arunachalam A

unread,
Mar 9, 2010, 11:18:32 AM3/9/10
to material...@googlegroups.com
Sorry, I did not see the items for which this is used. For valves, it is acceptable to use ASTM, in place of SA.
arun

GOPU NAIR

unread,
Mar 9, 2010, 11:47:09 PM3/9/10
to material...@googlegroups.com
Dear Muthu
 
There are few differences between SA material and ASTM material.  If you require SA216 material, please refer to the Sec. II Part A 2007 Edition and read the fine print under the ASME Monogram which reads (Identical with ASTM A216/A 216M-93 except for the addition of 2.3 and editorial differences in 2.1 and 10.1)
 
For any material please refer to such fine prints.  However, this is mostly applicable when the product has to be code stamped.Test certificate to be reviewed for compliance with SA material including the year and recertification is also to be done.
 
Hope this clarifies your doubts. 
 Regards
 
Gopu Nair

--- On Tue, 9/3/10, vijay frnds <frndst...@gmail.com> wrote:

From: vijay frnds <frndst...@gmail.com>
Subject: [MW:4502] ASTM A216 Vs ASME SA216 Difference
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.
Reply all
Reply to author
Forward
0 new messages