> Hi,
>
> Can anybody suggest what tests must be conducted to check welding quality
> of Duplex SS.
> Is there any European standard for these tests details.
>
> BR,
>
> Pankaj Johri, GradIEAust,
>
> ___________________________________________________________________________ ____________________________________
>
> This e-mail communication (and any attachment/s) may contain confidential
> or privileged information and is intended only for the individual(s) or
> entity named above and to others who have been specifically authorized to
> receive it. If you are not the intended recipient, please do not read,
> copy, use or disclose the contents of this communication to others. Please
> notify the sender that you have received this e-mail in error by reply
> e-mail, and delete the e-mail subsequently. Please note that in order to
> protect the security of our information systems an AntiSPAM solution is in
> use and will browse through incoming emails.
> Thank you.
> ___________________________________________________________________________ ______________________________________
>
> Ce message (ainsi que le(s) fichier(s)), transmis par courriel, peut
> contenir des renseignements confidentiels ou protégés et est destiné à
> l?usage exclusif du destinataire ci-dessus. Toute autre personne est, par
> les présentes, avisée qu?il est strictement interdit de le diffuser, le
> distribuer ou le reproduire. Si vous l?avez reçu par inadvertance,
X-ray test is preferred. EN 1435/ EN 25817, UT may be applied EN 1714/ EN
1712 (Level 2 or B)
TRAN VAN VUONG
Brg,
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to
materials-weld...@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.